Specify fogging, VOC emissions and heat ageing separately when buying aftermarket silicone parts for vehicle interiors. Approve the production compound, colour and cure on finished parts, then check fit and function after the agreed heat exposure.
Key Sourcing Takeaways
- Name the method, revision, specimen and acceptance limit on the RFQ.
- Include production pigments, markings, adhesives and any post-cure in the approval sample plan.
- Check fit and function after heat exposure in the installed condition.
Four-Stage Lot Inspection & Raw-to-Shipment Traceability
- 01
Material grade & batch COA
- 02
Mixing & molding records
- 03
2D optical FAI records
- 04
SGS/TÜV finished-part scope

Put three separate checks on the drawing
| Concern | Specify for the test | Check at approval |
|---|---|---|
| Fogging on glass | DIN 75201 procedure where required by the buyer, including the specimen and conditioning | Record the reported reflectance or condensate mass and the matching buyer limit |
| VOC emissions | Buyer-specified emission method, sample age and any post-cure | Match reported quantities, units and sample identification to the specification |
| Heat ageing | Exposure duration and temperature, mounting load, cooling interval and properties to measure | Retest fit, recovery or retention at the interface that matters |
DIN 75201 addresses fogging of vehicle interior materials. Confirm the procedure and revision with the buyer before sending samples.
VDA 278 uses thermal desorption to characterize organic emissions from non-metallic vehicle materials. It reports VOC and FOG values under its test conditions. Ask the buyer to specify any separate glass fogging, odour or vehicle air quality tests.
ISO 188 provides accelerated ageing and heat-resistance methods for rubbers. Define the functional checks for the installed part separately. A single oven exposure gives results for that exposure and the properties measured.
Choose samples that represent the part buyers will receive
Use production-intent silicone with the specified pigment, print, adhesive and cure. Agree whether each test uses an intact part or a specimen cut from it. Send the lab the compound lot, moulding date, sample mass or exposed area, conditioning instructions and any post-cure record. Ask the buyer which formulation or process changes trigger resubmission.
Recheck the interface after heat
For a console liner, inspect edge lift and slide resistance with the actual tray. For a key-fob cover, check button clearance and return with the remote installed. For a connector dust cap, inspect retention and the contact witness against the mating housing. Define the exposure and cooling interval in advance, and use the same fixture for before and after measurements.