Engineering Tool 01 · ASTM D2240 / ISO 7619-1 Durometer Reference
Silicone Shore Hardness Chart (Shore 00, Shore A & Shore D)
Use our interactive durometer selector and conversion table to match 10A–80A silicone compounds to real-world tactile feel, part wall thickness, and LSR vs. HCR molding capabilities.
Complete Durometer Conversion & Application Table
Silicone Shore 00, Shore A (10A–80A) & Shore D Engineering Reference
Youbang compounds custom Shore A durometers from 0–80A (30–70A most common) on 2 in-house mixing mills with outgoing Shore A durometer verification.
| Shore A | Shore 00 | Shore D | Everyday Feel Equivalent | Preferred Process | Representative Silicone Applications |
|---|---|---|---|---|---|
| 10 Shore A | 55–60 Shore 00 | — | Similar to soft gel insoles or jelly candy; stretches and conforms effortlessly | Low-viscosity 2-part platinum LSR injection | Vibration-damping gel pads, medical tissue simulators, ultra-soft acoustic ear tips |
| 20 Shore A | 70 Shore 00 | — | Comparable to a gummy bear; gentle low-pressure skin seal | 85T / 120T LSR liquid injection molding | Respiratory mask cushion skirts, nasal pillows, deep-undercut 3D artisan candle molds |
| 30 Shore A | 80 Shore 00 | 6 Shore D | Comparable to a soft rubber band or baby bottle nipple; folds and snaps back cleanly | LSR injection (preferred) or tear-resistant HCR | Sensitive-bladder LSR menstrual cups, soft-tip baby spoons, intricate chocolate & soap molds |
| 40 Shore A | 86 Shore 00 | 9 Shore D | Comparable to a pencil eraser; balances velvet flexibility with self-supporting walls | Both LSR injection and 200–250T HCR compression | Standard LSR menstrual cups (40–45A), oral teethers, baby bibs, collapsible bowl hinge zones |
| 50 Shore A | 90 Shore 00 | 12 Shore D | Comparable to a car wiper blade; balanced compression-set recovery and tear strength | HCR compression / LSR injection / P+R keypad overmolding | Waterproof housing gaskets & O-rings, P+R keypad tactile webbing, suction baby plates, pet lick mats |
| 60 Shore A | 93 Shore 00 | 16 Shore D | Comparable to a bicycle inner tube; resists sagging across wide spans | 200–250T large-platen HCR compression | Kitchen sink drying mats, pet maze slow-feeders, rugged POS/scanner protective sleeves, pastry pans |
| 70 Shore A | 96 Shore 00 | 22 Shore D | Comparable to a car tire tread or running-shoe outsole; firm load support | HCR compression (Silicone, EPDM, NBR or FKM) | Steel-rod roll-up rack end tracks, high-pressure flange seals, furniture leg caps, firm spatula blades |
| 80 Shore A | 98 Shore 00 | 30 Shore D | Comparable to a hard leather shoe heel; minimal finger indentation | High-durometer HCR compression (generous draft angles required) | Heavy machinery bump stops, rigid snap-fit grommets, industrial anti-vibration mounting pucks |
Sourcing & Tooling FAQ
Key Answers Before Tooling
Covering CAD readiness, custom MOQ evaluation, free 3D fit checks vs. T1 silicone samples, NDA protection and mold ownership.
Send your drawing or sample photo directly to Zhou Li’s engineering desk for a 24h DFM reply.
What is the standard manufacturing tolerance for Shore A hardness on custom silicone parts?+
Industry-standard custom molding tolerance is ±5 Shore A (verified per ASTM D2240 / ISO 7619-1 on flat ≥ 6 mm stacked test buttons or plied sections). Tighter compound lot control (such as ±3 Shore A) can be evaluated per project during raw-material compounding.
Why do two parts with the same 50 Shore A durometer feel softer or firmer in the hand?+
Apparent stiffness depends heavily on wall thickness and rib geometry—a 0.8 mm thin-wall 50A menstrual cup rim feels supple and foldable, whereas a 6 mm solid 50A bumper puck feels noticeably firm. We recommend verifying geometry with 1–3 free 3D prototypes and confirming tactile rebound on molded T1 samples.
Which Shore A hardness is best for baby tableware, menstrual cups, and waterproof gaskets?+
LSR menstrual cups typically use 30–45 Shore A; baby suction plates and spoons use 40–55 Shore A; waterproof housing gaskets and P+R keypads typically use 45–60 Shore A; and load-bearing kitchen drying mats or roll-up rack ends use 60–70 Shore A.
Can Youbang send physical Shore A sample chips before we lock our steel mold compound?+
Yes. We can ship existing-mold silicone reference parts across soft, medium and firm Shore A grades within 3–5 days (courier freight borne by the buyer) so your product team can feel actual elastomer rebound before T1 sampling.
B2B Factory Direct · 24h Engineering & Tooling Review
Need Tactile Advice or Existing-Mold Reference Samples?
Share your target product use and wall thickness—Zhou Li’s team will recommend the exact platinum LSR or HCR durometer within 24 hours.
Direct Dongguan Engineering Desk
- Accepts STEP / IGES / PDF / DWG or sample photos
- New mold T1 typically 7–15 days · Mass run 15–30 days
- Direct Tel / WeChat: +86 185 6655 6911 (Zhou Li)