Engineers designing orthotic heel inserts, delicate acoustic dampeners, or wrist rest pads often chase ultra-low Shore 00 durometer numbers straight off soft gel samples—only to hit sticky surfaces, oil seepage, torn molded ribs, and slow manual pouring quotes. Across Dongguan Youbang's 0–80 Shore A production capability (spanning 10 closed-loop 85T–160T LSR presses and 15 HCR vacuum lines), comparing bare Shore 00 gels against structured 10–20A platinum LSR saves painful post-tooling redesigns.

Materials & Regulatory ComplianceUpdated

4 min readCompiled by Youbang Silicone Engineering Team

Key Sourcing Takeaways

  • Open-poured Shore 00 silicone gels yield maximum vertical flesh-like pressure absorption, yet inherently suffer surface tack, low tear resistance, and potential silicone-oil plasticizer migration unless sealed inside protective TPU/PU films or coated fabrics.
  • Closed-loop 10–20 Shore A platinum LSR (molded across Youbang's 85T–160T injection systems) cures dry with micro-matte EDM cavity finishes or soft-touch coatings—holding sharp honeycombs, perimeter ribs, and snap lips without oil bleeding.
  • By shifting wall architecture from solid slabs to collapsible honeycomb grids, open cells, or ribbed skirts, 10–20A molded LSR frequently matches the perceived fingertip squish of Shore 00 gel at far cleaner cycle consistency and durability.

Poured Shore 00 Silicone Gel vs. 10–20 Shore A Closed-Loop Platinum LSR

Poured Shore 00 Silicone Gel vs. 10–20 Shore A Closed-Loop Platinum LSREngineering process control benchmark · final tolerances confirmed per project CADProcess parameter window (verified per part CAD)Open-Poured Shore 00 Silicone Gel• Maximum flesh-like sag under low vertical load• Inherent surface tack; oil-bleed risk without pouch• Low tear strength; unstable thin ribs or undercuts• Slow open casting; awkward naked demolding10–20A Soft LSR (0–80A Line)• Crisp hollow cells & micro-ribs off 85T–160T LSR• Dry matte skin + tactile coat; zero oil exudation• Reliable snap recovery & much higher tear safety• Pair hollow ribs to mimic Shore 00 feel at lower costUse hollow-rib 10–20A platinum LSR instead of bare Shore 00 gel whenever dry demold matters
Engineering process control benchmark · final tolerances confirmed per project CAD
Dry matte pale sky-blue molded 15 Shore A LSR honeycomb cushion pad beside a glossy soft poured Shore 00 gel block and analog durometer on a QC mat
Dry matte pale sky-blue molded 15 Shore A LSR honeycomb cushion pad beside a glossy soft poured Shore 00 gel block and analog durometer on a QC mat

When industrial and wellness product teams hold an existing retail heel cup or delicate shock pad, two radically different elastomer families often get lumped together under one casual label—"super-soft silicone." In production reality, open-poured Shore 00 silicone gel and molded 10–20 Shore A platinum LSR behave completely differently on steel parting lines, inside retail boxes, and across repeated washings.

Operating across 0–80 Shore A elastomers inside our 8,000 m² Dongguan plant (10 closed-loop LSR presses and 15 vacuum HCR presses), our tooling engineers walk buyers through four key trade-offs before picking a hardness specification.

1. Material Physics & Processing Reality Check

Reserve Shore 00 gels for encapsulated low-shear bladders; switch exposed, washable, or ribbed parts to structured 10–20 Shore A platinum LSR.

Decision Dimension Open-Poured Shore 00 Silicone Gel Molded 10–20 Shore A Platinum LSR (0–80A Window) Engineering & Retail Packaging Impact
Surface Feel & Dust Cling Naturally tacky jelly surface; readily grabs hair/lint unless sealed inside TPU film Dry silky matte skin straight from micro-EDM steel (optionally paired with cured soft-touch coat) Exposed heel cushions and wearable bands stay clean in everyday travel bags
Oil Bleed / Exudation Risk High low-molecular oil load risks yellowing/staining adjacent paper or suede shoe linings Full 200 °C × 4–6h circulating oven baking clears volatiles (≤0.5% target) Critical for retail cardboard sleeves, apparel inserts, and sensitive electronics
Rib & Undercut Definition Weak tensile tear resistance; sharp internal cells easily rip during demolding High-elongation platinum LSR replicates crisp honeycombs, perimeter flanges & button walls cleanly Enables repeatable ±0.05 mm fit lands and predictable snap assemblies
Cycle Economics & Scale Manual pot-pouring or slow gravity dispensing limits multi-cavity automation Automated closed-loop 85T–160T metering delivers uniform multi-cavity shots from 100 pcs to volume scale Predictable piece-price amortization (15–30 day mass-production turns)

2. Achieving Shore 00 Perceived Plushness Using Geometry Instead of Oil-Heavy Gels

Think of compressibility as Material Modulus × Structural Void Fraction:

  1. Instead of pouring a 12 mm solid slab of sticky Shore 00 gel, tool a 15–20 Shore A platinum LSR honeycomb matrix or slanted flexing wall.
  2. Under foot or ergonomic contact, those hollow columns buckle smoothly at low force—replicating the exact soft sink-in profile buyers want while keeping all external skins non-tacky, tear-tough, and dishwasher/soap washable.

3. Qualifying Durometer Comfort Across 100 pcs Physical Trials

Never finalize soft-elastomer hardness purely from a desktop Shore calculator:

  • Confirm frame/housing envelope clearance on free 3D-printed structural prototypes (buyer pays freight).
  • Test real compression deflection, lint cling, and wash recovery on 7–15 day T1 molded samples starting from 100 pcs pilot runs across two candidate durometers (for example, 15A vs. 25A hollow-rib sections).

Explore our medical & wellness silicone family or vibration damper mounts for a first hardness-to-geometry review within 24 hours.

References & Engineering Sources

  1. Dongguan Youbang 0–80 Shore A Capabilities & Medical/Health Molding Lines
  2. ASTM D2240 — Standard Test Method for Rubber Property—Durometer Hardness
Turn the selection into a reviewable project brief

Sourcing & Tooling FAQ

Key Answers Before Tooling

Covering CAD readiness, 100 pc trial & 1,000 pc / $2,000 USD standard MOQ policy, free 3D fit prototypes vs. T1 silicone samples, NDA protection, and mold ownership.

Have a part-specific question?

Send your drawing or sample photo directly to Youbang’s engineering desk; we send an initial response within 24 hours.

Why do bare ultra-soft Shore 00 silicone gel blocks attract dust instantly or leave greasy rings on paper packaging?

Most Shore 00 gels rely on heavily extended, very low crosslink-density silicone oil fractions to stay jelly-soft—causing natural surface tack and gradual oil migration unless laminated inside TPU pouches or washed/coated thoroughly.

Can Dongguan Youbang injection-mold clean mechanical ribs and thin walls at 10–20 Shore A without tearing on demold?

Yes—across controlled 85T–160T closed-loop platinum LSR systems paired with polished steel cavities and matched draft angles, stable low-durometer 10–20 Shore A cushions demold reliably within our broader 0–80 Shore A capability window.

How can designers make a 15–20 Shore A molded part feel as plush under heel or wrist load as solid Shore 00 gel?

Replace solid rubber thickness with vertical collapsible buckling ribs, ventilated honeycomb columns, or hollow vacuum-relieved domes—letting structural geometry provide soft compressive spring while high-tear platinum LSR supplies skin-dry recovery.

What sample sizes support testing tactile softness before locking steel production molds?

After verifying overall footprint with free 3D geometry prototypes (buyer pays freight), trial LSR or HCR runs start cleanly from 100 pcs within 7–15 days post-tooling so product teams compare live skin tack and compression feel directly.

B2B Factory Direct · initial response within 24 hours

Test Shore 10A–20A vs. hollow-rib soft cushioning geometry at T1

Share cushioning deflection load, skin-contact vs. encapsulated housing conditions, and STEP CAD for elastomer & rib-layout guidance within 24 hours.

✓ Trial from 100 pcs · Standard 1,000 pcs or $2,000 USD✓ Free 3D-printed fit prototypes before steel tooling✓ Paid molds 100% owned by customer

Send Your Project Brief or CAD

For confidential drawings, sign the mutual NDA before uploading the files.

Only rights holders or their authorized representatives may upload files. We keep inquiries and attachments to prepare quotes and follow up on your project.

Prefer email or files > 20 MB? Send directly to zhouli@ybsilicone.com · Privacy Policy